Diagnosis before treatment
Stain diagnosis
Ten kinds of marking, the giveaway that identifies each one, what to treat it with and â the part that saves floors â what will make it permanent. Two of the ten are not stains at all, and they are the two most often treated as if they were.
Guided diagnosis
Choose what best matches what you are looking at and the tool narrows it to a marking. The full table is below and needs no tool.
All ten markings are in the full table below, which works without the script.
First, decide which of three things you are looking at
Hold a torch at a low angle across the surface and look along it rather than down at it.
- A stain is colour that has moved into the stone. The surface still reflects evenly; the colour is wrong. Treatment pulls it back out.
- An etch is colour that has not changed at all while the surface has been dissolved by acid. It looks dull, feels very slightly rough, and appears and disappears as you move your head. Treatment re-polishes it.
- Efflorescence is salt arriving from behind the stone, as a white powder that comes back after each sweep. Treatment is to find the water that is carrying it; nothing applied to the face will stop it.
The table
| Marking | Giveaway | Treat with | Never |
|---|---|---|---|
| Oil and grease | Dark patch with a soft feathered edge; often larger than the original spill and darker on a warm day | LOOP-R3 mixed with a mild solvent, 6 mm thick, 48 hours; up to three applications | Scrub with a degreaser â it drives the oil deeper. Seal over it while the area is still damp |
| Organic: tea, coffee, leaves, wine | Pinkish to tan brown, holding the outline of the spill or the leaf | LOOP-R3 with 12 % hydrogen peroxide, 24 hours | Use household bleach on coloured or dark stone; it can lighten the stone more than the stain |
| Etch marks and dull rings | Colour unchanged; the shine is missing and the mark appears only at certain angles | LOOP-P2, white pad, 90-second passes | Apply more cleaner, or anything sold as an acidic «stain remover» â that is what caused it |
| Hard-water deposit | Crusty off-white build-up around taps and shower bases, slightly raised to a fingernail | Plastic scraper first, then LOOP-N4 at 1:20, repeated over several days | Use a limescale remover. Every one of them is acidic and will etch calcite stone within seconds |
| Rust and iron | Orange-brown, in the exact shape of the object that sat there, or as spots following the veining | An iron-specific poultice from a restoration supplier. We do not blend one | Poultice it with peroxide: it oxidises the iron further and sets the colour permanently |
| Efflorescence | White powder that returns within days of sweeping, usually on floors under a year old | Dry brushing, repeated weekly, while the source of moisture is traced and stopped | Wash it off with water. You dissolve the salt, it soaks back in and returns with company |
| Ink and dye | Sharp-edged, intense colour, often with a visible stroke or splash shape | LOOP-R3 with peroxide on pale stone, with a mild solvent on dark stone; test on an offcut first | Use acetone on filled travertine or a resin-backed slab â it softens the filler and the backing resin |
| Paint | Sits on top of the stone, has thickness, and catches a fingernail | A plastic blade to lift the bulk, then LOOP-R3 with a mild solvent on the residue only | Use alkaline paint stripper on polished marble; it leaves a pale burn that needs re-polishing |
| Biological growth | Pink or black film in permanently damp areas; slimy rather than gritty | LOOP-N4 at 1:20, then fix the ventilation or the standing water | Rely on repeated chlorine: it bleaches cement-based grout and keeps coming back while the damp remains |
| Copper and bronze runs | Green to brown streaks running downwards from a metal fitting | A specialist metal-stain poultice. Expect partial removal at best, and replace or isolate the fitting | Reach for acid. It will etch the stone and leave the metal salts exactly where they were |
Three mistakes we hear about every month
Treating an etch as a stain
Somebody spends a fortnight applying stronger and stronger cleaners to a dull ring that no cleaner can touch, and by the end the whole area around it is also dulled. The etch guide starts with a torch test precisely because of this.
Sealing to hide something
A sealer is not a coating and it will not darken a mark into invisibility. What it will do is trap the mark under a layer that now has to be removed before anything else can be tried. Diagnose, treat, let it dry for 48 hours, then seal.
Starting on the visible area
Every treatment on this page should be proved on an offcut, inside a cupboard or under an appliance first. Two slabs cut from the same block can behave differently, and the only way to find out is somewhere nobody will look.
When to stop and call a restoration contractor
- The damage is deeper than about half a millimetre â you can catch it with a fingernail rather than just feel a change in texture.
- An etched area is larger than roughly a quarter of the surface. Re-polishing patches will leave a visible map; at that point the whole surface wants honing and polishing as one job.
- The stone is cracked, hollow-sounding or lifting. That is a bedding and substrate problem, and no product on this site is relevant to it.
- It is iron staining that has come from inside the stone. It is not coming out, and the useful conversation is about replacement.
If you are unsure which row you are in, email info@marbleloop.cloud with a photograph taken at a low angle, one taken straight on, and the age of the installation. Those three things settle most of it.